MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Saint-Gobain COHRlastic® 700 General Purpose Silicone Solid Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durometer to the relatively hard 70 durometer on the Shore A scale. It is manufactured in different formulations to provide a choice of physical properties and cost considerations. Series 300-700: COHRlastic general-purpose molded sheet is available in thicknesses up to 1/2" and it withstands temperatures from -100°F to +500°F. RED in color.All data based on a 0.25 inch test sample.(Also comes in thicknesses from 1/16" to 1/2")
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 65 - 7565 - 75Increases by 5 after dry heat aging for 70 hrs at 437°F.; ASTM D2240
Tensile Strength, Yield 4.83 MPa700 psiTensile strength decreases by 15% after dry heat aging for 70 hrs at 437°F.; ASTM D412
Elongation at Break 160 %160 %Elongation properties decrease by 15% after dry heat aging for 70 hrs at 437°F.; ASTM D412
Tear Strength 10.5 kN/m60.0 pliInitial Tear Strength; ASTM D624
Compression Set 15 %
@Temperature 160 °C
15 %
@Temperature 320 °F
Constant Deflection, 70 hrs.; ASTM D395
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 19.7 kV/mm500 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 270 µm/m-°C
@Temperature 20.0 °C
150 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 1.26 J/g-°C0.300 BTU/lb-°F
Thermal Conductivity 0.187 W/m-K1.30 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain COHRlastic® 600 General Purpose Silicone Solid Rubber
Overview of materials for Silicone Rubber
Wacker Elastosil® LR 3003/60 A/B Liquid Silicone Rubber
CHT Group QM 261 60 Shore A, Addition Cure Moldmaking Material
Saint-Gobain COHRlastic® 500 General Purpose Silicone Solid Rubber

PSTGQZ234 / 68748

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.