MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Superior Flux Superior No. 530 Bromide-Based Tube Mill Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Continuous Brass Tinning Flux for Radiator Brass Tube Mill
  • Extremely Fast Tinning Properties
  • Draws Strong Internal Joint for Lockseam Tube Mill
  • Leaves No Residue After Tinning
  • Has Excellent Oil Absorption Properties
  • 100% Bromide, No Clean Formulation Uses No Corrosive Chloride
Description: Superior No. 530 is a bromide-based, inorganic acid type flux, specifically designed for brass tube mill soldering. The unique mix of fluxing ingredients of Superior No. 530 flux offers a high degree of fluxing activity and excellent oil absorption, both essential properties for brass tube mill soldering. Superior No. 530 leaves virtually no residue in lockseam tubes.

Applications: Superior No. 530 was formulated specifically for continuous soldering in a radiator tube mill, either welded or lockseam type. The Superior No. 530 formulation has been designed to completely remove the excessive water-oil mix used for brass tube mill material lubrication. Normal flux application is total immersion of the brass tube.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.078 - 1.098 g/cc
Density 9.10 lb/gal
Surface Tension 32 dynes/cm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 260 - 427 °CSoldering Range
Shelf Life 2.00 Month
 
Descriptive Properties
AppearanceClear, Red
Free Acid11.2-15.2%HBr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for AISI 4000 Series Steel

NSFLUX073 / 185757

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.