MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® A3Z BK 30464 PA66 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Description: Impact-modified and stabilized injection- molding grade for components and housings with good low temperature impact resistance.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 - 0.800 g/cc
Density 1.06 g/ccISO 1183
Moisture Absorption at Equilibrium 2.0 - 2.6 %23°C; 50% RH; ISO 62
Water Absorption at Saturation 6.7 - 7.7 %ISO 62
Linear Mold Shrinkage 0.0085 cm/cmrestricted
Melt Flow 10.6 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 40.0 MPa50 mm/min; ISO 527-1/-2
Elongation at Break 18 %Nominal, 50mm/min; ISO 527-1/-2
Modulus of Elasticity 0.850 GPaISO 527-1/-2
Izod Impact, Notched (ISO) 50.0 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 NB
@Temperature 23.0 °C
ISO 180/A
Charpy Impact Unnotched NBISO 179/1eU
Charpy Impact, Notched NB
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohmIEC 60093
Dielectric Constant 3.6
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.070
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VTest solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.330 W/m-KDIN 52612
Melting Point 260 °CDIN 53765
Decomposition Temperature >= 310 °C
Ignition Temperature >= 400 °CASTM D1929
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 °CHopper Throat
Zone 1 290 °CFeed zone
Zone 2 290 °CCompression
Zone 3 290 °CMetering-zone
Zone 4 290 °CNozzle
Melt Temperature 280 - 300 °CInjection-molding/Extrusion
 290 °COptimal
Mold Temperature 40.0 - 80.0 °CInjection-molding
 60.0 °COptimal
Drying Temperature 80.0 °C
Dry Time 4 hour
Moisture Content 0.030 - 0.060 %Optimal
 <= 0.15 %
 
Descriptive Properties
ColorBK 30464
Commercial StatusEurope
Peripheral Screw Speed< 0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® A3Z HP PA66 (Dry)
BASF Basotect UL Foam
BASF Ultradur® B 4040 G10 BK5110 50% Glass Filled PBT
BASF Ultramid® 1000-11 NF2001 PA66 (Conditioned)
BASF Ultramid® A3Z BK 30464 PA66 (Dry)

PBASG0225 / 131858

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.