MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Interior South Douglas Fir Wood
Categories: Wood and Natural Products; Wood; Softwood

Key Words: Pseudotsuga Menziesii; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.450 g/cc0.450 g/ccGreen, based on volume
 0.460 g/cc0.460 g/cc12% moisture content, based on volume
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 1601 N359.9 lb (f)Green
 2224 N500.0 lb (f)12% moisture content
Tensile Strength at Break 1.72 MPa250 psiGreen, perpendicular to grain
 2.28 MPa330 psi12% moisture content, perpendicular to grain
Modulus of Elasticity 8.00 GPa1160 ksiGreen
 10.3 GPa1490 ksi12% moisture content
Modulus of Rupture 0.0469 GPa6.80 ksiGreen
 0.0820 GPa11.9 ksi12% moisture content
Compressive Strength 2.34 MPa340 psiGreen, perpendicular to grain
 5.10 MPa740 psi12% moisture content, perpendicular to grain
 21.4 MPa3110 psiGreen, parallel to grain
 43.0 MPa6230 psi12% moisture content, parallel to grain
Shear Strength 6.55 MPa950 psiGreen, parallel to grain
 10.4 MPa1510 psi12% moisture content, parallel to grain
Impact 1515Impact bending in inches, green
 2020Impact bending in inches, 12% moisture content
Work to Maximum Load 0.0552 J/cm³8.00 in-lb/in³Green
 0.0621 J/cm³9.00 in-lb/in³12% moisture content

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Coast Douglas Fir Wood
American Rocky Mountain Douglas Fir Wood
Interior West Douglas Fir Wood
Interior North Douglas Fir Wood
Douglas-fir Plywood

PTSU002 / 71444

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.