MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mid-Mountain Materials THERMOSEAL® FIBERPAK® T22 Tamping Mix
Categories: Ceramic

Material Notes: Description: THERMOSEAL® T22 FIBERPAK® TAMPING MIX is a wet taping mix made up of bulk refractory fibers and a high temperature binder system. T22 FIBERPAK® TAMPING MIX is particularly good for use in forming light weight and rigid insulating structures such as boiler door linings, covers, hoods and various furnace backup linings. T22 FIBERPAK® TAMPING MIX is resistant to the attack of most chemicals with the exception of hydrofluoric and phosphoric acids and strong alkalis. It is totally unaffected by thermal shock and has very low heat transfer.

APPLICATION: Use THERMOSEAL® T22 FIBERPAK® TAMPING MIX as packaged. Place into mold or area to be filled, and hand or mechanically tamp in place to assure void removal and adequate compaction. Allow for drainage of excess binder through mess screen or weep hole. Air dry or force dry bellow 500ºF • 260ºC.

PACKAGING: THERMOSEAL® T22 FIBERPAK® TAMPING MIX is available in five gallon plastic buckets and 55 gallon drums. T22 is available winterized to protect from freezing in cold climates. Do NOT allow T22 FIBERPAK® TAMPING MIX to freeze.

Information provided by Mid-Mountain Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.320 - 0.400 g/cc0.0116 - 0.0145 lb/in³Dried Density (Depending on Tamp Density)
 1.12 - 1.20 g/cc0.0405 - 0.0434 lb/in³Wet Density (Depending on Tamp Density)
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.000310 GPa0.0450 ksi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1260 °C2300 °FUse Limit
Shrinkage  2.0 %
@Temperature 982 °C,
Time 86400 sec
2.0 %
@Temperature 1800 °F,
Time 24.0 hour
 5.0 %
@Temperature 1260 °C,
Time 86400 sec
5.0 %
@Temperature 2300 °F,
Time 24.0 hour
 
Descriptive Properties
ColorOff-White
CompositionAlumina 22%, Silica 78%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMID60 / 1564

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.