MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Rigid Molding M5730  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.32 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cmASTM D955
Spiral Flow 88.9 cmRelative Spiral Flow; 23
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 79
@Time 15.0 sec
ASTM D2240
Tensile Strength, Yield 42.7 MPaType I, 51 mm/min; ASTM D638
Elongation at Break 50 %Type I, 51 mm/min; ASTM D638
Tensile Modulus 2340 MPaType I, 51 mm/min; ASTM D638
Flexural Strength 71.0 MPaASTM D790
Flexural Modulus 2410 MPaASTM D790
Izod Impact, Notched 53.4 J/m
@Thickness 3.18 mm,
Temperature -18.0 °C
Injection Molded; ASTM D256A
 267 J/m
@Thickness 3.18 mm,
Temperature 0.000 °C
Injection Molded; ASTM D256A
 427 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 73.9 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
 77.8 °C
@Thickness 6.35 mm
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
 76.1 °C
@Thickness 6.35 mm
Annealed; ASTM D648
UL RTI, Electrical 50.0 °CUL 746
UL RTI, Mechanical with Impact 50.0 °CUL 746
UL RTI, Mechanical without Impact 50.0 °CUL 746
Flammability, UL94 V-0
@Thickness 1.60 mm
All colors; UL 94
 5VA
@Thickness 1.91 mm
All colors; UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 199 - 210 °C
 
Descriptive Properties
FeaturesGeneral Purpose
 High Flow
 Medium Impact Resistance
FormsPellets
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesConstruction Applications
 General Purpose
 Outdoor Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Rigid Molding M5700 Natural Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Rigid Molding M5730 Natural Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Rigid Molding M5700
Geon® Performance Solutions Vinyl Fittings M1015 Polyvinyl Chloride, Rigid

PH1PN8865 / 102701

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.