MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SACO AEI EXTINITY® 0101-108 Halogenated, Flame Retardant Compound
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: EXTINITY® 0101-108 is a halogenated, flame retardant compound specifically designed for use in plenum tube applications. This compound has good thermal stability and can be converted easily on standard processing equipment.

Recommended Applications:
Film: Cast
Molding: Injection, Compression
Extrusion: Sheet, Tubing, Jacketing

Information provided by SACO AEI Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 g/ccASTM D792
Melt Flow 0.60 g/10 minASTM D1238 Condition E
Storage Temperature 40.0 - 80.0 °F
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 2500 psiASTM D638
Tensile Strength, Yield 1600 psiASTM D638
Elongation at Break 650 %ASTM D638
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -55.0 °CASTM D746
Flammability, UL94 V-2
@Thickness 1.27 mm
Oxygen Index 27 %ASTM D746
 
Processing PropertiesOriginal ValueComments
Zone 1 280 - 310 °F
Zone 2 300 - 340 °F
Zone 3 320 - 360 °F
Zone 4 320 - 360 °F
Die Temperature 330 - 370 °F
Melt Temperature 320 - 340 °F
Head Temperature 330 - 370 °F
 
Descriptive Properties
FormNatural Pellets
Horizontal Flame TestPass50 mil
Stress Crack Resistance048 hrs, ASTM D1693

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSACO022 / 249389

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.