MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Starguide™ ISO 46
Categories: Fluid; Lubricant

Material Notes: Texaco Starguide oils deliver value through:
  • Cleaner cutting — Reduce excessive drag that slows cutting.
  • Exceptional performance for low water and low oil consumption saw systems.
  • Excellent low temperature properties — Low pour point and proprietary formulation keep guide holes, lines and filters free from build-up associated with low temperatures.
  • Rust and corrosion protection
  • Excellent lubrication due to oily film on saw blade
  • Operator comfort — Low odor
  • Environmental sensitivity — The severely hydrotreated mineral oil and ashless additive formulation has passed aquatic toxicity tests under EPA and European Union criteria and is considered "nontoxic". These tests include the industry accepted LC-50 tests which measures toxicity to rainbow trout, daphnia shrimp, and green algae.

Texaco Starguide oils are designed to promote longer saw guide and saw blade life in thin kerf saw equipment, when operating in severe service and reduced cooling water modes.

Texaco Starguide oils are formulated with Group II base stocks and specially selected ashless additives to reduce friction between saw and guide components in thin kerf saw equipment.

The oil lubricity performance minimizes rust and corrosion problems, while reducing friction to allow much cooler operation.

Texaco Starguide oils have been formulated with effective rust inhibitors to prevent rust formation.

Oiliness and EP properties provide excellent film strength for boundary lubrication and extreme pressure conditions.

Texaco Starguide oils have the optimum emulsification to allow the correct mixing of oil and water and have tackiness properties to enable the lubricants to cling to saw and guide components.

Texaco Starguide oils are specifically formulated to lubricate modern thin kerf sawing systems. Original Equipment Manufacturers and sawmill customers were consulted prior to product design and laboratory testing. Texaco Starguide oils performance properties have been field proven to meet the severe requirements of this application.

Texaco Starguide oils meet or exceed the performance requirements of most saw system manufacturers, including: CAE (Newnes, McGehee), Optimil, Salem, TMT, Ukiah, and USNR (Kockums CanCar, Schurman).

Texaco Starguide ISO 46 is recommended for and has been used successfully in band saw mist applications.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 256000; MSDS Number: 9011

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 32 °
Viscosity Measurement 118Viscosity Index
Saybolt Viscosity at 100°F 224 SUS
Saybolt Viscosity at 210°F 50 SUS
Kinematic Viscosity at 40°C (104°F) 43.7 cSt
Kinematic Viscosity at 100°C (212°F) 7.0 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point -33.0 °C
Flash Point 242 °C
 
Descriptive Properties
Rust PreventionPass24 h

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WTEXA176 / 77055

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.