MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Industeel URANUS® B66 High Strength Super-Austenitic Stainless Steel with PREN = 54
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T S30000 Series Stainless Steel

Material Notes: Description: Research carried out these last five years has shown that combined additions of chromium, tungsten, molybdenum, nitrogen and copper, make it possible to design a super-austenitic stainless steel with mechanical properties equivalent to the alloy 625 and with very high corrosion resistance properties. Due to 22% Ni and 0.4% N additions, the new URANUS® B66 (UR B66) alloy exhibits a very stable microstructure, less prone to intermetallic phase precipitations than the other highly alloyed austenitic stainless steels. The UR B66 alloy has improved corrosion resistance properties compared to 6 Mo grades particularly in sea water and chlorinated sea water. Due to the optimum "cocktail" of alloying elements, the grade can be used in most very severe corrosive environments where it behaves almost equivalent or better than alloy 625.

Information provided by manufacturer.

Key Words: EURONORM (X1 Ni Cr Mo Cu 22.24.6), AFNOR (Z2 CNDWU 24.22.06.AZ), ASTM UNS S31266
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.20 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 220 - 260Typical, V10
Tensile Strength, Ultimate >= 750 MPaMinimum Guaranteed
Tensile Strength, Yield >= 420 MPa
@Strain 0.2 %
 >= 440 MPa
@Strain 1 %
Elongation at Break >= 50 %
Modulus of Elasticity 195 GPa
Poissons Ratio 0.30Calculated
Shear Modulus 75.0 GPa
@Temperature 20.0 °C
Charpy Impact >= 100 J
@Temperature -196 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000100 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.0 µm/m-°C
@Temperature 20.0 - 100 °C
 16.0 µm/m-°C
@Temperature 20.0 - 300 °C
 16.5 µm/m-°C
@Temperature 20.0 - 500 °C
Specific Heat Capacity 0.450 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 12.0 W/m-K
@Temperature 20.0 °C
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 24 %
Copper, Cu 1.5 %
Iron, Fe <= 41.1 %As remainder
Manganese, Mn 3.0 %
Molybdenum, Mo 6.0 %
Nickel, Ni 22 %
Nitrogen, N >= 0.40 %
Tungsten, W 2.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carlson 904L Austenitic Stainless Steel
Carlson 926 Mo Austenitic Stainless Steel
Crucible Steel SUE52 Martensitic Steel
Industeel URANUS® B26 6 Mo High Performance Super-Austenitic Stainless Steel with PREN = 43
Industeel URANUS® B28 High Nickel Super-Austenitic Stainless Steel

NINDUST45 / 17583

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.