MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum 7021-T62
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A97021; Aluminium 7021-T62; AA7021-T62; Al7021-T62
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.78 g/ccAA; Typical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 112500 kg load with 10 mm ball. Calculated value.
Hardness, Knoop 140Converted from Brinell Hardness Value
Hardness, Rockwell A 44.8Converted from Brinell Hardness Value
Hardness, Rockwell B 70Converted from Brinell Hardness Value
Hardness, Vickers 127Converted from Brinell Hardness Value
Tensile Strength, Ultimate 420 MPa
Tensile Strength, Yield 380 MPa
Elongation at Break 13 %
@Thickness 1.60 mm
In 5 cm
Modulus of Elasticity 72.0 GPaAverage of Tension and Compression. In Al alloys, the compressive modulus is typically 2% greater than the tensile modulus. Estimated from trends in similar Al alloys.
Poissons Ratio 0.33Estimated from trends in similar Al alloys.
Fatigue Strength 140 MPa
@# of Cycles 5.00e+8
Shear Modulus 27.0 GPaEstimated from similar Al alloys.
Shear Strength 250 MPaCalculated value.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000450 ohm-cmEstimated from trends in similar Al alloys.
 
Thermal PropertiesOriginal ValueComments
CTE, linear 23.6 µm/m-°C
@Temperature 20.0 - 100 °C
 25.3 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.880 J/g-°CEstimated from trends in similar Al alloys.
Thermal Conductivity 140 W/m-KEstimated from trends in similar Al alloys.
Melting Point <= 640 °CEstimated from trends in similar Al alloys.
Liquidus 640 °CEstimated from trends in similar Al alloys.
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 90.7 - 93.7 %As remainder
Chromium, Cr <= 0.05 %
Copper, Cu <= 0.25 %
Iron, Fe <= 0.40 %
Magnesium, Mg 1.2 - 1.8 %
Manganese, Mn <= 0.10 %
Other, each <= 0.05 %
Other, total <= 0.15 %
Silicon, Si <= 0.25 %
Titanium, Ti <= 0.10 %
Zinc, Zn 5.0 - 6.0 %
Zirconium, Zr 0.08 - 0.18 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
7020-T6 Aluminum
Aluminum 7029-T5
7020-T652 Aluminum
Aluminum 7075-T6; 7075-T651
Aluminum 7034-T6

MA7021T62 / 9548

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.