MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Amodel® A-1230 L Polyphthalamide (PPA)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), Mineral Filled

Material Notes: Amodel A-1230 L is a 30% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and tensile strength, and low moisture absorption. - Black: A-1230 L BK 324

Additional Information: Continuous Use Temperature, ASTM D3045, 5000 hrs: 311°F Continuous Use Temperature, ASTM D3045, 20000 hrs: 275°F

Data is presented for dry polymer.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 g/ccISO 1183/A
Filler Content 30 %Mineral Filler
Water Absorption 0.12 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.011 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.011 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 126R-Scale; ASTM D785
Tensile Strength, Yield 95.8 MPaISO 527-2
 104 MPaASTM D638
Elongation at Break 1.6 %ASTM D638
 1.6 %ISO 527-2
Tensile Modulus 6890 MPaISO 527-2
Flexural Yield Strength 200 MPaASTM D790
Flexural Modulus 6210 MPaASTM D790
Compressive Strength 152 MPaASTM D695
Poissons Ratio 0.31ASTM E132
Shear Modulus 2.63 GPaCalculated
Shear Strength 81.4 MPaASTM D732
Izod Impact, Notched 43.0 J/mASTM D256
Charpy Impact Unnotched 25.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 2.10 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.9
@Frequency 1e+6 Hz
ASTM D150
 4.2
@Frequency 60 Hz
ASTM D150
Dielectric Strength 21.0 kV/mm
@Thickness 3.18 mm
ASTM D149
Dissipation Factor 0.0060
@Frequency 60 Hz
ASTM D150
 0.018
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 125 secASTM D495
Comparative Tracking Index 550 VUL 746
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 41.0 µm/m-°C
@Temperature 0.000 - 100 °C
TMA; ASTM E831
 88.0 µm/m-°C
@Temperature 160 - 249 °C
TMA; ASTM E831
CTE, linear, Transverse to Flow 49.0 µm/m-°C
@Temperature 0.000 - 100 °C
ASTM E831
 110 µm/m-°C
@Temperature 160 - 249 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 279 °CUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 158 °CUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 3.18 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 304 - 318 °C
Front Barrel Temperature 316 - 329 °C
Melt Temperature 321 - 343 °C
Mold Temperature 135 °C
Drying Temperature 120 °C
Dry Time 2.50 hour
Moisture Content 0.045 %
 
Descriptive Properties
AdditiveLubricant
 Mold Release
AppearanceBlack
AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
FeaturesGood Chemical Resistance
 Low Moisture Absorption
 Low Warpage
 Lubricated
FormsPellets
GenericPPA
Processing MethodInjection Molding
RoHS ComplianceRoHS Compliant
UsesAutomotive Applications
 Electrical/Electronic Applications
 Industrial Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polyplastics Duranex® 3316 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 30% GF filled
Celanese Zytel® FR50 BK505 PA66-GF25FR(17)
Celanese Zytel® 45HSB NC010 PA66
Polyplastics Duranex® 3300H Polybutylene Terephthalate (PBT), Standard, 30% GF filled
Nilit Polynil® P240HSLV High Viscosity, Heat Stabilized Nylon 66

PSOL8Y7515 / 135594

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.