MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Tungsten Alloy A97
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: Applications include nuclear and medical radiation shielding for x-ray and radiation therapy shields and industrial applications, aircraft and helicopter rotor balance weights, instrument balance weights, weights for sport equipment, tool damping cutter bars, and high voltage contacts.

Data provided by MarkeTech International

Vendors: Elmet Technologies is a 100% US owned and operated, fully integrated manufacturer of Molybdenum, Tungsten and related alloys such as TZM, WHA & MoLa. At our 220,000 sqr/ft plant in Lewiston, Maine, Elmet manufactures W & Mo pure powders plus rod, wire, plate, sheet & foil in additional to offering fabrication and machining services. ITAR, ISO and AS9100 registered. www.elmettechnologies.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 18.6 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 31
Tensile Strength, Ultimate 882 MPa
Tensile Strength, Yield 735 MPa
Elongation at Break 5.0 %in 25 mm
 
Component Elements PropertiesOriginal ValueComments
Iron, Fe 1.5 %from NiFe binder
Nickel, Ni 1.5 %from NiFe binder
Tungsten, W 97 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tungsten Alloy A90
Tungsten Alloy A93
WNiFe Class 1 Tungsten Alloy
Tungsten Alloy A95
WNiFe Class 3 Tungsten Alloy

MWAER6 / 14285

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.