MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phillips 66 Syndustrial® Rotary Compressor Oil ISO Grade 32/46
Categories: Fluid; Lubricant; Polyglycol

Material Notes: Syndustrial Rotary Compressor Oil is a premium quality, readily biodegradable synthetic lubricant developed for use in centrifugal and rotary air compressors. It is particularly recommended for use in applications where operating conditions are unfavorable or too severe for conventional mineral oil-based compressor oils. Syndustrial Rotary Compressor Oil is formulated with a blend of synthetic polyalkylene glycol (PAG) and synthetic ester base oils and carefully selected additives. It has outstanding oxidation resistance and thermal stability at high temperatures to minimize deposit formation and provide long service life. It has high film strength to protect against wear, and also protects against rust and corrosion. It is classified as readily biodegradable, as defined by the OECD 301B test method, for reduced environmental impact in case of leaks or spills. It also passes the visual “no sheen” requirements of the U.S. EPA Static Sheen Test (Federal Register Vol. 58, No. 41). Syndustrial Rotary Compressor Oil is formulated to outperform conventional paraffinic or naphthenic compressor oils in oxidation resistance and deposit control. It has better thermal stability at high temperatures to minimize sludge and varnish formation. It also has lower volatility for lower oil consumption. These benefits result in longer service intervals and less maintenance than with conventional petroleum oils.

Applications:

  • Centrifugal air compressors and oil-flooded rotary screw, rotary lobe and rotary vane air compressors where the manufacturer specifies a synthetic polyglycol/ester lubricant
  • Drop-in replacement for OEM-branded polyglycol-based compressor oils
Features/Benefits:
  • Outstanding oxidation resistance and thermal stability at high temperatures
  • High viscosity index and very low pour point for use over a wide temperature range
  • Excellent cooling and heat transfer properties
  • Excellent deposit control
  • High film strength for wear protection
  • Low volatility for lower oil consumption and less makeup oil
  • Protects against rust and corrosion
  • Extended service intervals compared with mineral oil-based lubricants
  • Readily biodegradable for reduced environmental impact in case of leaks or spills
  • Compatible with commonly used seals, gaskets and hoses

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.964 g/cc
Density 8.03 lb/gal
Viscosity Measurement 174Index
Saybolt Viscosity at 100°F 182 SUS
Saybolt Viscosity at 210°F 50.6 SUS
Kinematic Viscosity at 40°C (104°F) 35.9 cSt
Kinematic Viscosity at 100°C (212°F) 7.3 cSt
Oxidative Stability >= 30 hourRPVOT; ASTM D2272
ASTM Color 0.50ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.17[mg KOH/g]; ASTM D974
 
Mechanical PropertiesOriginal ValueComments
Four Ball Wear 0.530 mmScar Diameter; ASTM D4172
 
Thermal PropertiesOriginal ValueComments
Pour Point -57.0 °C
Flash Point 251 °CCOC
 
Descriptive Properties
Biodegradability>90%28 days, OECD 301B
Copper Corrosion1aASTM D130

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5044 / 198297

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.