MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem GM5010T2U Extrusion High Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Description: GM5010T2U is a High Density Polyethylene compound with high molar mass specially developed for the manufacturing of jacketing of umbilicals. It is produced with bimodal technology, shows high mechanical properties and has excellent resistance to stress cracking. GM5010T2U contains carbon black pigment that protects it against ultraviolet radiation action and photodegradation.

Application: Jacketing of umbilicals, risers and flowlines for oil field platforms.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.955 g/ccASTM D792
ESCR 100% Igepal® >= 1000 hour
@Temperature 50.0 °C
F50, molded 2 mm, 0.3 mm notched-plaques; ASTM D1693
Oxidative Induction Time (OIT) >= 50 min
@Temperature 200 °C
ASTM D3895
Carbon Black Loading 2.3 - 2.7 %ASTM D1603
Melt Flow 0.45 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62ASTM D2240
Tensile Strength at Break 34.0 MPaASTM D638
Tensile Strength, Yield 23.0 MPaASTM D638
Elongation at Break 800 %ASTM D638
Elongation at Yield 9.1 %ASTM D638
Flexural Modulus, 1% Secant 1090 MPaASTM D790
Izod Impact, Notched 220 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °CASTM D648
Vicat Softening Point 124 °C
@Load 1.02 kg
ASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Extruded
Braskem GP5550BK HDPE High Density Extrusion Polyethylene
Braskem GD5150K HDPE High Density Extrusion Polyethylene
Borealis Borstar® CB9600 HDPE for Extrusion Coating
Braskem GP5550 HDPE High Density Extrusion Polyethylene

PBRASK2076 / 199957

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.