MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik TEGOMER® E 525 Dispersing additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product description: TEGOMER® E 525 is a dispersing additive especially designed for the preparation of polyethylene color concentrates and filler compounds based on PE or PP.

Application: TEGOMER® E 525 is a highly efficient dispersing aid for color concentrates based on polyethylene as a carrier. TEGOMER® E 525 is applicable for mono or tailor made color concentrates and highly filled compounds. It is recommended for the use for film, injection and molding application. Benefits: The following advantages can be expected when TEGOMER® E 525 is used:

  • increase of color strength
  • higher productivity and lower costs for coloration
  • high filling grades of pigments
  • excellent clarity and reduction of speck formation in films or thin moulded parts
  • less agglomerates and aggregates
  • excellent dilution behavior
  • suppression of re-agglomeration in down-stream processes

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 200 cPmelt
 
Mechanical PropertiesOriginal ValueComments
Penetration 5.0[dmm]
 
Thermal PropertiesOriginal ValueComments
Dropping Point 96.0 °C
 
Descriptive Properties
Appearancefree flowing powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik TEGOMER® DA 800 Dispersing additive
BCC Products MB 1100 Polyurethane Foam Modeling Board

PEVONIL583 / 196787

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.