MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman Diamond ASA M-143
Categories: Polymer; Thermoplastic; ASA Polymer; Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded

Material Notes: Description: ASA Weatherable Polymer, Injection Molding Grade, High Heat

Information provided by Diamond Polymers, Inc.

A. Schulman has acquired Network Polymers & Diamond Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D955
Melt Flow 4.4 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Procedure A Condition G; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 7672 psichs 2 in/min; ASTM D638
Flexural Strength 11600 psichs 0.05 in/min; ASTM 790
Flexural Modulus 355000 psiTangent, chs 0.05 in/min; ASTM D790
Izod Impact, Notched 1.70 ft-lb/in
@Thickness 3.17 mm,
Temperature 23.0 °C
bar; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 203 °F0.125 in bar Unannealed/Conditioned 40 hours at 23°C; ASTM D648
 217 °F0.25 in bar Unannealed/Conditioned 40 hours at 23°C; ASTM D648
Vicat Softening Point 248 °F0.125 inch, 1 Kg; ASTM D1525
 
Optical PropertiesOriginal ValueComments
Gloss 96.5 %at 60°; ASTM D523
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 480 - 490 °F
Middle Barrel Temperature 500 - 510 °F
Front Barrel Temperature 510 - 520 °F
Nozzle Temperature 510 - 520 °F
Melt Temperature 430 - 520 °FMelt temperatures above 530°F are not recommended, and may result in color shifts and or thermal instability.
Mold Temperature 170 - 180 °FHigher mold temperature can aid flow in processing, provides a better surface finish, and creates less residual stress in the finished products.
Drying Temperature 180 - 198 °F
Dry Time 4 - 6 hour
Moisture Content <= 0.10 %
Back Pressure 75.0 - 150 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Diamond ASA 91802
A. Schulman Diamond ASA 5946
A. Schulman Diamond ASA S150
A. Schulman Diamond ASA S210B
A. Schulman Diamond ASA S-150E-1115 ASA Weatherable Polymers Extrusion Grade, Medium Impact

PDIAM267 / 30105

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.