MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 1385 C TFE 15 Z Polyphenylene Sulfide (PPS) Carbon Fiber - PTFE Lubricated - FDA Compliant Ingredients  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes:

Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.54 g/cc1.54 g/ccASTM D 792
Additive Loading 30 %30 %Primary Additive
Linear Mold Shrinkage 0.00050 - 0.0015 cm/cm
@Thickness 3.20 mm
0.00050 - 0.0015 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 165 MPa24000 psiASTM D 638
Elongation at Break 1.0 - 2.5 %1.0 - 2.5 %ASTM D 638
Tensile Modulus 24.8 GPa3600 ksiASTM D 638
Flexural Strength 248 MPa36000 psiASTM D 790
Flexural Modulus 22.8 GPa3300 ksiASTM D 790
Izod Impact, Notched 0.587 J/cm
@Thickness 3.20 mm
1.10 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 3.74 J/cm
@Thickness 3.20 mm
7.00 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1000 ohm-cm<= 1000 ohm-cmASTM D 257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C500 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 307 - 329 °C585 - 625 °F
Mold Temperature 135 - 177 °C275 - 350 °F
Drying Temperature 149 °C
@Time 21600 sec
300 °F
@Time 6.00 hour
Moisture Content 0.040 %0.040 %
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 1385 D TFE 15 Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced - PTFE Lubricated
RTP Company RTP 1385 TFE 15 Polyphenylene Sulfide (PPS), Carbon Fiber - PTFE Lubricated
RTP Company RTP 1382 AR 10 TFE 15 Polyphenylene Sulfide (PPS) Carbon Fiber - Aramid Fiber - PTFE Lubricated
RTP Company RTP 1403 P TFE 10 Polyphenyl Sulfone (PPSU), Glass Fiber - PTFE Lubricated - Preliminary Data
Lehvoss LUVOCOM® 1301-7449 PPS, linear with carbon fiber and PTFE

PQZVA16494 / 120476

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.