MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 6003-55A Z Specialty Thermoplastic Elastomer, Bondable to PC/PMMA, PC/PBT
Categories: Polymer; Thermoplastic; Elastomer, TPE

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/ccASTM D 792
Linear Mold Shrinkage 0.015 - 0.018 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 5510 s delay; ASTM D 2240
Tensile Strength at Break 800 psi
@Thickness 3.17 mm
Die C; 20 in/min (500 mm/min); ASTM D412
Elongation at Break 1000 %
@Thickness 3.17 mm
Die C; 20 in/min (500 mm/min); ASTM D412
Tear Strength 175 pliDie C; ASTM D 624
Peel Strength 31.0 pliPC/PBT; Failure Type D; 90 degrees, 20 in/min (500 mm/min); ISO 813
 33.0 pliPC/PMMA; Failure Type D; 90 degrees, 20 in/min (500 mm/min); ISO 813
Compression Set 19 %
@Temperature 23.0 °C,
Time 79200 sec
Method B; Type 2; ASTM D 395
 65 %
@Temperature 70.0 °C,
Time 79200 sec
Method B; Type 2; ASTM D 395
 
Processing PropertiesOriginal ValueComments
Melt Temperature 380 - 460 °F
Mold Temperature 70.0 - 120 °F
Drying Temperature 170 °F
Dry Time 2 - 4 hour
Moisture Content <= 0.040 %
Injection Pressure 5000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 1899 A X 83675 Polycarbonate/Acrylic Alloy (PC/PMMA), Thin Wall Grade
Samyang Triloy® 120H PC/ABS alloy
Röhm CyRex® 100 Acrylic-Polycarbonate Alloy
Overview of materials for Polyetheretherketone, Unreinforced
Evonik CYREX® Protect Acrylic-polycarbonate alloy

PQZWA8505 / 92386

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.