MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Dyneon™ TF 2025Z PTFE Fine Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Dyneon™ TF 2025 Z PTFE is an ideal grade for pipe liner applications in chemical plant construction due to high green strength.

Product Features:

  • High molecular weight
  • Fine powder grade for low to medium reduction ratio
  • High stretch ratio
  • Processable by standard paste extrusion methods
  • Can be used for unsintered thread sealing tape, joint sealing and pipe lining, yarns and thick wall tubing
  • Meets ASTM D4895-04 Type 1, Grade 1, Class B classification

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.480 g/cc0.0173 lb/in³DIN EN ISO 60
Particle Size 500 µm500 µmaverage; ISO 13320
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 34.0 MPa4930 psiDIN EN ISO 527-3
Elongation at Break 360 %360 %DIN EN ISO 527-3
 
Descriptive Properties
Extrusion Pressure40 MPareduction ratio 400, ASTM D4894
Reduction Ratio Range20-300:1Dyneon Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC Fluon® CD123 PTFE Coagulated Dispersion Powder
Chemours Teflon® PTFE 640 Resin for Lubricated Paste Extrusion
Chemours Teflon® PTFE 65 Resin for Lubricated Paste Extrusion
3M Dyneon™ TF 2072 PTFE Paste Extrusion Powder
3M Dyneon™ TFM™ 1700 PTFE

PDYNE040A / 149079

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.