MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Rayon ACRYPET VR S40 001 PMMA Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Impact Modified, Molded

Material Notes: Good impact strength and good molding properties.

Typical Products: Interior parts of Auto mobile and Audio system. Indicator window of mobile phone.

Information provided by Mitsubishi Rayon Co.,Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/ccISO 1183; JIS K7112
Water Absorption 0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/inMRC method
Melt Flow 7.7 g/10 min
@Load 3.80 kg,
Temperature 230 °C
7.7 g/10 min
@Load 8.39 lb,
Temperature 446 °F
ISO 1133
Spiral Flow  190 cm
@Thickness 2.00 mm,
Temperature 250 °C
74.8 in
@Thickness 0.0787 in,
Temperature 482 °F
MRC method
 300 cm
@Thickness 2.00 mm,
Temperature 250 °C
118 in
@Thickness 0.0787 in,
Temperature 482 °F
MRC method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 5959ISO 2039
Tensile Strength 47.0 MPa6820 psi1A/5; ISO 527
Elongation at Break 15 %15 %1A/5; ISO 527
Modulus of Elasticity 1.90 GPa276 ksi1A/1; ISO 527
Flexural Strength 69.0 MPa10000 psiISO 178
Flexural Modulus 1.90 GPa276 ksiISO 178
Izod Impact, Unnotched (ISO) 9.20 kJ/m²4.38 ft-lb/in²1A; ISO 180
Charpy Impact Unnotched 15.0 J/cm²71.4 ft-lb/in²11eU; ISO 179
Charpy Impact, Notched 0.820 J/cm²3.90 ft-lb/in²1eA; ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1e+12 ohm-cm>= 1e+12 ohm-cmJIS K6911
Surface Resistance >= 1.00e+16 ohm>= 1.00e+16 ohmJIS K6911
Dielectric Constant 3.7
@Frequency 60 Hz
3.7
@Frequency 60 Hz
JIS K6911
Dielectric Strength 20.0 kV/mm508 kV/in4kV/sec; JIS K6911
Dissipation Factor 0.050
@Frequency 60 Hz
0.050
@Frequency 60 Hz
JIS K6911
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FASTM D696
Specific Heat Capacity 1.50 J/g-°C0.359 BTU/lb-°FJIS K7123
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C178 °FISO 75
Vicat Softening Point 87.0 °C
@Load 5.10 kg
189 °F
@Load 11.2 lb
ISO 75
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.49
@Wavelength 587.6 nm
1.49
@Wavelength 587.6 nm
nd; ASTM D542
Haze 0.50 %
@Thickness 3.00 mm
0.50 %
@Thickness 0.118 in
ISO 14782
Transmission, Visible 92 %
@Thickness 3.00 mm
92 %
@Thickness 0.118 in
ISO 13468
 
Descriptive Properties
Arc Resistanceno trackJIS K6911

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Rayon ACRYPET IR S404 001 PMMA Resin
Mitsubishi Rayon Acrypet® VH-001 Heat Stabilized PMMA
Mitsubishi Rayon ACRYPET MD 001 PMMA Resin
Mitsubishi Rayon Acrypet® MF 001 PMMA
Mitsubishi Rayon ACRYPET VH 000 PMMA Resin

PMITS9914 / 185889

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.