MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Renishaw 8060-3 Vacuum casting resin
Categories: Polymer; Thermoset

Material Notes: Description: Simulates PP/PE

Features: Resistant to high temperatures

Suitable for: Automotive, under bonnet/hood

Information provided by Renishaw

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/ccPart A
 1.21 g/ccPart B
Viscosity 50 cPPart B
 220 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80Cured; ISO 868
Flexural Strength 64.0 MPaCured; ISO 178
Flexural Modulus 1320 MPaCured; ISO 178
Izod Impact, Notched (ISO) 13.0 kJ/m²Cured; ISO 180
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 115 - 180 °CCured, (test piece 110 mm × 12.7 mm × 6.4 mm); ISO 75
Glass Transition Temp, Tg 125 - 195 °CCured
Shrinkage 0.50 %
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 °CResin Temp
Mold Temperature 70.0 °C
Cure Time 60.0 min
@Temperature 65.0 - 70.0 °C
Pot Life 330 sec
@Load 0.100 kg
 
Descriptive Properties
ColorSlightly yellow
Mixing ratio by weightA:B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Renishaw 8040 Vacuum casting resin
Renishaw 9012 Vacuum casting resin

PRENISH026 / 206389

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.