MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
FKuR Kunststoff Bio-Flex® F 1138 PLA Blend
Categories: Polymer; Film; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: The film extrusion grade Bio-Flex® F1138 is certified compostable according to EN 13432 and has been especially designed for the production of bags. The improved material characteristics, especially the increased tear resistance, allow reducing the thickness of the bags: It is possible to realize thicknesses down to 10µ. Shopping bags made from Bio-Flex® F 1138 are resilient enough to be reused several times, finally they can be used as a waste bag for organic waste collection. Biodegradable and compostable compound for film extrusion, certified according to EN 13432 with a maximum thickness of 60 µm. Used in applications such as T-shirt bags and waste bags.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.47 g/ccISO 1183
Melt Flow 2.0 - 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 14.0 MPaISO 527
Tensile Strength, Ultimate 16.0 MPaISO 527
Film Tensile Strength at Yield, MD 20.0 MPa
@Thickness 0.0300 mm
BUR 2.3; ISO 527
Film Tensile Strength at Yield, TD 14.0 MPa
@Thickness 0.0300 mm
BUR 2.3; ISO 527
Film Elongation at Break, MD 430 %
@Thickness 0.0300 mm
BUR 2.3; ISO 527
Film Elongation at Break, TD 470 %
@Thickness 0.0300 mm
BUR 2.3; ISO 527
Elongation at Break 370 %ISO 527
Modulus of Elasticity 0.405 GPaISO 527
Tensile Modulus 260 MPa
@Thickness 0.0300 mm
Film TD, BUR 2.3; ISO 527
 410 MPa
@Thickness 0.0300 mm
Film MD, BUR 2.3; ISO 527
Flexural Strength 10.0 MPa
@Strain 3.5 %
ISO 178
Flexural Modulus 390 MPaISO 178
Elmendorf Tear Strength, MD 5.10 g/mil
@Thickness 0.0300 mm
BUR 2.3; ASTM D 1922
Elmendorf Tear Strength, TD 25.5 g/mil
@Thickness 0.0300 mm
BUR 2.3; ASTM D 1922
Film Tensile Strength at Break, MD 20.0 MPa
@Thickness 0.0300 mm
BUR 2.3; ISO 527-3
Film Tensile Strength at Break, TD 13.0 MPa
@Thickness 0.0300 mm
BUR 2.3; ISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 155 °CISO 3146-C
 
Descriptive Properties
Bio-based carbon content (%)10ASTM D 6866
Certified Compostableyes
Spencer Impact Test (N/mm)200ASTM D 3420, BUR 2.3, 0.03mm thickness

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
FKuR Kunststoff Bio-Flex® F 1137 PLA Blend
FKuR Kunststoff Bio-Flex® F 5710 PLA Blend
FKuR Kunststoff Bio-Flex® FX 1120 PLA Blend
FKuR Kunststoff Bio-Flex® F 1804 Compostable PLA Blend
FKuR Kunststoff Bio-Flex® FX 1803 Compostable PLA Blend

PFKUR903 / 192723

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.