MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex ELEXAR® EL 8623 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Notes: Elexar® EL-8623 is high performance thermoplastic elastomer, available in BLK and NAT, designed for a variety of electrical including wire & cable. Elexar® EL-8623 is a high hardness, high density grade and is suitable for both injection molding and extrusion.

Features: Chemical Resistant, Filled; Flame Retardant; Good Adhesion; Good Colorability; Good Moldability; Good Processability; Good Toughness; High Density; High Hardness; Low Flow

Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire & Cable Applications; Wire Jacketing

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information provided by Teknor Apex Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/ccASTM D792
Melt Flow 4.5 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50
@Time 10.0 sec
ASTM D2240
 53
@Time 1.00 sec
ASTM D2240
Tensile Strength, Yield 2560 psiASTM D412
 2483.2 psi
@Treatment Temp. 136 °C,
Time 605000 sec
in Air; ASTM D573
 2529 psi
@Treatment Temp. 60.0 °C,
Time 605000 sec
in IRM 902 Oil; ASTM D471
Tensile Stress at Strain 1070 psi
@Strain 100 %
ASTM D412
 1340 psi
@Strain 300 %
ASTM D412
Elongation at Break 560 %ASTM D412
 511.84 %
@Treatment Temp. 136 °C,
Time 605000 sec
in Air; ASTM D573
 533.12 %
@Treatment Temp. 60.0 °C,
Time 605000 sec
in IRM 902 Oil; ASTM D471
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 9.70e+15 ohm-cm
@Temperature 50.0 °C
ASTM D257
Dielectric Constant 2.37
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 910 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -45.0 °CASTM D746
UL RTI, Electrical 194 °FUL 746
UL RTI, Mechanical with Impact 194 °FUL 746
Flammability, UL94 HB
@Thickness 0.762 mm
All Colors
Oxygen Index 23 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 390 - 420 °F
Middle Barrel Temperature 415 - 430 °F
Front Barrel Temperature 430 - 440 °F
Nozzle Temperature 430 - 445 °F
Zone 1 380 - 410 °F
Zone 2 390 - 420 °F
Zone 3 415 - 430 °F
Zone 4 415 - 430 °F
Zone 5 430 - 440 °F
Die Temperature 430 - 445 °F
Melt Temperature 430 - 445 °FProcessing Temp
Mold Temperature 77.0 - 150 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 50.0 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Aquathene® FR409800 Polyethylene Wire and Cable Compound
Teknor Apex ELEXAR® EL 8614 Thermoplastic Elastomer
Teknor Apex ELEXAR® EL 8451 Thermoplastic Elastomer
LyondellBasell Pro-fax 8623 Polypropylene Impact Copolymer
Teknor Apex ELEXAR® EL 8730 Thermoplastic Elastomer

PTEKNO264 / 70007

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.