MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kraton® D1101 J (SBS) Liner Block Copolymer
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: Kraton D1101 J is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Japan in the physical form(s) outlined in the following grade nomenclature:
D1101 JO - supplied as dusted crumb
D1101 JU - supplied as undusted crumb
D1101 JSM - supplied as powder dusted with amorphous silica

Region: Asia Pacific, Europe, Japan, North America and South America

Uses: Kraton D1101 J is used as a modifier of bitumen and polymers. It is also suitable as an ingredient in formulating compounds for footwear applications and may be used in formulating adhesives, sealants and coatings.

Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; and Roads and Roofing

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/cc
Volatiles <= 1.0 %
@Temperature 110 °C,
Time 7200 sec
Viscosity 3000 - 5000 cP25% Toluene Solution at 25°C; KM 06
Melt Flow <= 1.0 g/10 minISO 37
Ash >= 0.50 %JU; ISO 247
 >= 1.0 %JO; ISO 247
 >= 5.0 %JSM; ISO 247
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 72
@Time 30.0 sec
ISO 868
Tensile Strength 33.0 MPaISO 37
300% Modulus 0.00290 GPa
@Strain 300 %
ISO 37
 
Descriptive Properties
ContentBound Styrene31 percent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® D1101 A (SBS) Liner Block Copolymer
INEOS Styrolution K-Resin® KR03 Styrene Butadiene Copolymer (SBC)
Kraton® FG1901 + PA-6 blend (20/80)
Kraton® FG1901 + PBT blend (30/70)
Kraton® G1702 + PPE blend (20/80)

PKRA9806 / 132705

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.