MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Magnesium Alloys, General
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: These properties are typical of commercial magnesium alloys. Some properties, such as strength, impact, and hardness, vary too much for a reasonable generalization. See entries for individual alloys for more specific information.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.74 - 1.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 45.0 GPa
Poissons Ratio 0.35
Shear Modulus 17.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000500 - 0.0000175 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 370 J/g
CTE, linear 26.0 µm/m-°C
@Temperature 20.0 - 100 °C
 27.0 µm/m-°C
@Temperature 20.0 - 200 °C
 28.0 µm/m-°C
@Temperature 25.0 - 260 °C
Specific Heat Capacity 0.960 - 1.05 J/g-°C
Thermal Conductivity 45.0 - 135 W/m-K
Melting Point 470 - 650 °C
Solidus 470 - 650 °C
Liquidus 595 - 650 °C
 
Component Elements PropertiesOriginal ValueComments
Magnesium, Mg 85 - 100 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Magnesium, Mg; Extruded
Overview of materials for Magnesium Alloy
Magnesium, Mg; Sand Cast
Magnesium AE42-F, Die Cast
Magnesium AZ31B-F, Extruded Solid Shapes

MM0001 / 12289

Parkway Products

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.