MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Vanadium (V) Oxide, V2O5
Categories: Ceramic; Oxide

Material Notes: Yellow-brown orthorhombic crystals

Key Words: V2O5, Vanadium Pentoxide, Vanadium Oxide
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 3.35 g/cc
Molecular Weight 181.88 g/mol
 
Electrical PropertiesOriginal ValueComments
Magnetic Susceptibility 0.000128cm^3/mol
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 354.6 J/g
Melting Point 670 °C
Decomposition Temperature 1800 °C
 
Descriptive Properties
CAS Number1314-62-1
ColorYellow brown
Crystal StructureOrthorhombic

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials IGS3723 Insulating Glass Sealant
Nitinol - NiTi Shape Memory Alloy; High-Temperature Phase
MV Labs TB800 Tb4O7 Terbium(III,IV) oxide
Mo-Sci Corporation GL 0179 Borosilicate glass frit
Momentive Performance Materials IGS3719-D1 Insulating Glass Sealant, Gray

EINOR0959 / 4093

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.