MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Bergamid™ XP6042701 Polyamide 6 (Nylon 6)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3.5 sec Cycle Time: 18 to 60 sec

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.43 g/ccASTM D792
Filler Content 10 %Carbon Fiber Reinforcement
 30 %Glass Fiber Reinforcement
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 165 MPaASTM D638
Flexural Modulus 9000 MPaASTM D790
Charpy Impact, Notched 90.0 J/cm²J/m; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Surface Resistance <= 1.00e+9 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 215 °CUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 230 - 240 °C
Middle Barrel Temperature 230 - 250 °C
Front Barrel Temperature 240 - 260 °C
Nozzle Temperature 240 - 260 °C
Mold Temperature 70.0 - 90.0 °C
Drying Temperature 100 - 110 °C
Dry Time 4.00 - 6.00 hour
Injection Pressure 100 - 150 MPa
Hold Pressure 50.0 - 80.0 MPa
Back Pressure 0.300 - 0.500 MPa
Screw Speed 80 - 160 rpm
 
Descriptive Properties
FormsPellets
Generic MaterialNylon 6
Generic NamePolyamide 6 (Nylon 6)
Processing MethodInjection Molding
Regional AvailabilityAsia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Niche Polymer POLIXL™ PA66GF33N PA66, 33% Fiberglass Reinforced, DAM
Hanwha Azdel Plus U400-B01N 41.5% Directionalized Continuous Fiber Mat / PP Resin Matrix
Domo TECHNYL® C 216 V35 Black Z PA6, 35% glass fiber, DRY
BASF Ultrason® E 2010 G6 30% Glass Filled PES
BASF Ultradur® B 4406 G6 Q717 30% Glass Filled PBT

PH0POL1311 / 145880

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.