MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Celcon® MC90-HM POM, Mineral Reinforced
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Mineral Filled

Material Notes: Celcon« MC90-HM is a highly mineral filled and coupled M90 material for producing very flat and dimensionally stable parts (normal flow).

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.60 g/ccASTM D792
Density 1.57 g/ccISO 1183
Moisture Absorption 0.200 %23°C/50%RH; ISO 62
Water Absorption at Saturation 0.75 %ISO 62
Linear Mold Shrinkage, Flow 0.015 cm/cmISO 294-4
 0.015 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.012 cm/cmASTM D955
 0.013 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 45.0 MPa50mm/min; ISO 527-2/1A
 6400 psiASTM D638
Elongation at Yield 6.0 %50mm/min; ISO 527-2/1A
Tensile Modulus 3550 MPa50mm/min; ISO 527-2/1A
Flexural Strength 72.0 MPaISO 178
Flexural Modulus 3500 MPaISO 178
 500000 psiASTM D790
Izod Impact, Notched 1.20 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 6.10 kJ/m²ISO 180/1A
Charpy Impact, Notched 6.30 kJ/m²ISO 179/1eA
 4.90 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°CISO 11359-2
Melting Point 165 °C10°C/min; ISO 11357-1,-2,-3
 329 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 103 °CISO 75-1, -2
 207 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 - 120 °Ccavity
 190 - 200 °Chot runner
Zone 1 170 - 180 °C
Zone 2 180 - 190 °C
Zone 3 180 - 190 °C
Zone 4 190 - 200 °C
Die Temperature 190 - 200 °C
Melt Temperature 180 - 200 °C
Drying Temperature 80.0 - 100 °C
Dry Time 3.00 hour
Injection Pressure 60.0 - 120 MPa
Hold Pressure 60.0 - 120 MPa
Back Pressure <= 4.00 MPa
 
Descriptive Properties
Injection moldingYes
Injection speedslow
PelletsYes
Processing conditions acc. ISO9988-2
Profile extrusionNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celcon® MC90 POM, Mineral Reinforced
A. Schulman Lucent POM-500 Acetal Homopolymer, General Purpose, Injection Grade
Delrin Delrin® 500AL NC010 POM-S
Master Bond MB297 Ethyl Cyanoacrylate Adhesive System
LG Chemical LUCEL MR-320 Low Warpage POM, 20% Mineral Filled

PHCQ136 / 178591

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.