MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chesterton 389 Synthetic Tapping Compound  (discontinued **)
Categories: Fluid

Material Notes: Description: Chesterton® 389 Synthetic Tapping Compound is a high performance, synthetic metal working fluid. It provides the industrial performance of conventional petroleum and solvent based fluids while eliminating the hazards normally associated with these traditional products. The superior lubrication of a synthetic, combined with maximum heat dissipating capability at the shear plane, results in a product which extends tool life and keeps taps cool to permit rapid cutting. Chesterton 389 is effective for all hand and automatic tapping operations and is used for a variety of demanding metal cutting operations over a broad range of metals, including aluminum. True and precise thread cutting action permits excellent thread quality. Ideal for dry seal threads and high pressure hydraulic fittings. Since ther is no chlorine or sulfur in the product, the working of stainless steel is facilitated without fear of embrittlement. Chesterton 389 is user and environmentally friendly. It is biodegradable, nonflammable and essentially odorless. Synthetic Tapping Compound does not smoke, mist or fume during use. The result is a cleaner, safer work environment. A near neutral pH minimizes the potential for skin irritation and defatting commonly caused by organic solvent based cutting fluids.

Features:

    Performance-
  • Excellent Lubricity
  • Superior Heat Dissipation
  • Reduced Galling
  • Extends Tool Life
  • Corrosion Inhibited
    Safety-
  • No chlorine, Chlorinated Hydrocarbons or Sulfur
  • Does Not Smoke, Fume or Mist
  • Essentially Odorless
  • Biodegradable

Suggested Uses:

    Operations-
  • Tapping
  • Boring
  • Reaming
  • Threading
  • Drilling
  • Milling
    Metals-
  • Stainless Steel
  • Aluminum
  • Brass
  • Bronze
  • Cast Iron
  • High Alloy Steel
  • Copper
  • Carbon Steel
  • Titanium
  • Titanium
  • Monel
  • Hastelloy

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/cc
pH 8.2
 
Thermal PropertiesOriginal ValueComments
Melting Point 0.000 °CFreezing Point
 
Descriptive Properties
AppearanceHazy, Yellow Color
FormViscous Liquid
Lubricity1100 kgFailure Load, ASTM D3233
 59 cm-kgFinal Torque, ASTM D3233
Reaction time>15 hrs
Tappin Torque Efficiency1.01vs. petroleum oil cutting fluids

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carlson C 625 Nickel-Chromium-Molybdenum Alloy
Haynes Hastelloy® G-30® alloy, 30% cold rolled
Haynes Hastelloy® B-3® alloy, 0% cold work
Chesterton 390 Cutting Oil
MetalTek MTEK N-7M Cast UNS N30007 Severe Corrosion and Heat Resistant Alloy

PPTCHS114 / 138226

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.