MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Thermoseal

(Viewing data as-entered. Click here to return)
Klinger Thermoseal Sealex® PTFE Tape Joint Sealant
Categories: Polymer; Tape; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Uses: Fume ducts. Concrete lids. Glass joints. Heat exchangers. Fiberglass reinforced plastic vessels. Pump or compressor housing flanges. Steam vessel flanges. Ceramic joints. Water systems. Valves and piping. Sealex joint sealant can be used wherever reliable gasketing is required. Sealex® joint sealant, specially processed, 100% pure PTFE on a roll, provides soft, highly compressible gasketing for longer life and trouble-free sealing. Its form-in-place versatility also cuts maintenance and storage costs. The high compressibility of Sealex® enables it to effectively fill flange imperfections for a tight, leak-free seal. Under pressure, it provides a very wide, thin ribbon-like joint sealant. Unlike conventional PTFE which is prone to cold flow, Sealex® has good creep resistance and bolt torque retention properties Sealex joint sealant does not support bacterial growth or cause product contamination and is FDA compliant. It has virtually no shelf-life concerns since PTFE is unaffected by normal environmental conditions. Sealex has excellent resistance properties to chemical attack. It works for most chemical services at temperatures to 500°F (260°C) and pressure to 2,000 psi (138 bar). The sealant is available in roll form in a wide variety of thicknesses and lengths.

Information provided by Thermoseal Inc.

Vendors: Thermoseal Inc. is the exclusive North American producer of Klinger Fluid Sealing products, including popular lines: Sealex, Klingersil and Topchem and our new Performance Technology Group of products. Visit us at Thermosealinc.com or call 1-800-990-7325 to speak with a fluid sealing specialist.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Apparent Bulk Density 0.600 g/cc
Solubility 0.00 ppminsoluble in water/grease
 
Thermal PropertiesOriginal ValueComments
Melting Point 325 - 335 °C
Maximum Service Temperature, Inert 500 °F
Minimum Service Temperature, Air -321 °F
Decomposition Temperature >= 375 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Colorgreycut edge
 white or blacksurface

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Superwool® Plus Textiles Braided Packing Thermal Ceramic
Rogers Arlon LW201B##-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported)
Overview of materials for Duplex
Special Metals INCONEL® Alloy 600
Saint-Gobain Norton® Fluorglas® Chemfilm® DF1400 Non-Conductive PTFE Tape

PTHERM955 / 192643

Thermoseal

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.