MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carlson C 625 Nickel-Chromium-Molybdenum Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: General Description

Carlson Alloy C 625 is a nickel-chromium-molybdenum alloy that combines high strength and oxidation resistance with excellent corrosion resistance. C 625 exhibits exceptional fatigue strength and superior strength and toughness over a wide temperature range – from cryogenic to approximately 1800°F (980°C)

The combination of high chromium and molybdenum provides excellent elevated temperature properties and outstanding aqueous corrosion resistance in a wide range of environments. Molybdenum also makes C 625 virtually immune to pitting and crevice attack in sea water and similar chloride environments.

The high nickel content of C625 provides immunity to chloride stress corrosion cracking.

C 625 is resistant to a number of corrosive environments, including sea water, phosphoric acid, organic acids, mixtures of oxidizing and reducing acids, caustic solutions and other aggressive chemicals encountered in pollution control environments.

Applications

C 625 is utilized in both high temperature and corrosive applications in chemical processing, pulp and paper, air pollution control, ore processing, waste treatment and disposal, steel pickling, marine equipment, nuclear reactor components, aerospace and gas turbines.

  • Chemical Process Equipment – Phosphoric acid, nitric-sulfuric and nitric-hydrofluoric acids, hydrofluoric and fluosilicic acid mixtures, sulfuric acid, calcium chloride and magnesium chloride, pesticides, and styrene.
  • Pulp and Paper – head boxes
  • Air Pollution Control – power plant scrubbers, electrostatic precipitators, waste-heat recovery systems, smelting scrubbers, and scrubbers for industrial boilers and inert-gas generators.
  • Ore Processing – uranium processing, copper refining, aluminum sulfate production.
  • Waste Treatment and Disposal – municipal refuse incinerators, sewage sludge incinerators, chemical and toxic waste incinerators.
  • Steel Pickling – hydrochloric acid
  • Marine Equipment – scrubbers for inert-gas generators, submerged equipment.
  • Aerospace and Gas Turbines – jet engine components, turbine blades.

Information provided by Carlson

Key Words: UNS N06625
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.44 g/cc0.305 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 758 MPa>= 110000 psi
Tensile Strength, Yield >= 379 MPa
@Strain 0.2 %
>= 55000 psi
@Strain 0.2 %
Elongation at Break >= 30 %>= 30 %
 
Electrical PropertiesMetricEnglishComments
Magnetic Permeability 1.00061.0006200 Oersted
Curie Temperature <= -195.56 °C<= -320.01 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  13.1 µm/m-°C
@Temperature 21.1 - 204 °C
7.30 µin/in-°F
@Temperature 70.0 - 400 °F
 13.7 µm/m-°C
@Temperature 21.1 - 427 °C
7.60 µin/in-°F
@Temperature 70.0 - 800 °F
 15.8 µm/m-°C
@Temperature 21.1 - 871 °C
8.80 µin/in-°F
@Temperature 70.0 - 1600 °F
Specific Heat Capacity 0.410 J/g-°C0.0980 BTU/lb-°F
Melting Point 1290 - 1350 °C2350 - 2460 °F
Solidus 1290 °C2350 °F
Liquidus 1350 °C2460 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.40 %<= 0.40 %
Carbon, C <= 0.10 %<= 0.10 %
Chromium, Cr 20 - 23 %20 - 23 %
Cobalt, Co <= 1.0 %<= 1.0 %
Iron, Fe <= 5.0 %<= 5.0 %
Manganese, Mn <= 0.50 %<= 0.50 %
Molybdenum, Mo 8.0 - 10 %8.0 - 10 %
Nb + Ta 3.15 - 4.15 %3.15 - 4.15 %
Nickel, Ni >= 58 %>= 58 %
Phosphorus, P <= 0.015 %<= 0.015 %
Silicon, Si <= 0.50 %<= 0.50 %
Sulfur, S <= 0.015 %<= 0.015 %
Titanium, Ti <= 0.40 %<= 0.40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals INCONEL® Alloy 625
ATI Allvac® Nickelvac® 625 Nickel Superalloy, Heat Treatment: 927°C (1700°F) Anneal
Chesterton 389 Synthetic Tapping Compound
Chesterton 390 Cutting Oil
Haynes Hastelloy® B-3® alloy, 0% cold work

NCARLSO20 / 15827

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.