MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman POLYBATCH™ ABPP-05 Antiblock Concentrate
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Description

POLYBATCH® ABPP-05 Antiblock is an antiblock concentrate containing 5% synthetic silica based in homopolymer polypropylene. This masterbatch is designed to provide high clarity, low haze, optimum dispersion, and consistent COF development when used in the skin layers of cast, blown and BOPP film applications. POLYBATCH® ABPP-05 is generally recommended for use at 2 to 3% addition levels depending upon customer specific requirements.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.930 g/ccASTM D792
Moisture Absorption 0.100 %190°C; ASTM D789
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
Ash 5.0 %ASTM D2765
 
Descriptive Properties
Pellet Count 45pellets/gram

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman POLYBATCH™ Woodland Green 30233U/4 Concentrate Based In LLDPE
Overview of materials for Polypropylene, Extrusion Grade
Overview of materials for Styrene/Butadiene/Styrene (SBS)
A. Schulman POLYBATCH™ Bright White LL80250 Concentrate Based In LLDPE
A. Schulman POLYBATCH™ AC-20531L UV Absorber Concentrate

PASHU361 / 25325

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.