MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
INEOS Styrolution Terblend® N NM-13 ABS/PA6 (Dry)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend; Nylon (Polyamide PA)

Material Notes: Terblend® N NM-13 is an ABS/PA blend with excellent impact toughness, especially at low temperature. Very high impact strength, High impact toughness at low temperature. Applications: Freezer parts, Ski top layers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccISO 1183
Moisture Absorption at Equilibrium 1.1 %
@Temperature 23.0 °C
50% RH; ISO 62
Water Absorption at Saturation 1.65 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage 0.0080 cm/cmISO 294-4
Melt Flow 25 g/10 min
@Load 10.0 kg,
Temperature 220 °C
Volumetric; cm3/10 min; ISO 1133
 25 g/10 min
@Load 10.0 kg,
Temperature 240 °C
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 35.0 MPaISO 527
Elongation at Break >= 50 %ISO 527
Elongation at Yield 3.4 %ISO 527
Tensile Modulus 1600 MPaISO 527
Flexural Strength 50.0 MPaISO 178
Flexural Modulus 1500 MPaISO 178
Izod Impact, Notched (ISO) 30.0 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 75.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact, Notched 30.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 80.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Dielectric Constant 2.9
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.015
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear >= 100 µm/m-°CISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °Cannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °Cannealed 4 hours at 80°C; ISO 75
Vicat Softening Point 91.0 °C
@Load 5.10 kg
VST/B/50. 50C/h; ISO 306
 165 °C
@Load 1.02 kg
VST/A/50. 50C/h; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 270 °CISO 294
Mold Temperature 40.0 - 80.0 °CISO 294
 
Descriptive Properties
Commercial StatusActive America
Primary Processing TechniqueInjection Molding
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Daicel CEVIAN® A1700 PA/ABS Alloy, DAM
Techmer ES Plastiblend® ABS/PA 1700
INEOS Styrolution Terblend® N NMX04 ABS/PA6 (Dry)
INEOS Styrolution Terblend® N NM-11 ABS/PA6 (Conditioned)
INEOS Styrolution Terblend® N NM-11 ABS/PA6 (Dry)

PBASF9044 / 84808

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.