MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI 4130H Steel, normalized at 870°C (1600°F)
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 4000 Series Steel; Low Alloy Steel; Carbon Steel; Medium Carbon Steel

Material Notes: A very common general purpose grade of medium carbon, Cr-Mo steel. Flexibility afforded by heat treatment options allows it to attain a range of toughness and strength values. Good hardenability, strength, wear resistance, toughness, and ductility.

Key Words: AFNOR 25 CD 4 (S), JIS SCM2, JIS SCCrM 1, SS14 2225 (Sweden), alloy steels, UNS H41300, ASTM A304, SAE J1268, DIN 1.7218, medium carbon steels, chromium-molybdenum, chrome-moly
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 197
Hardness, Knoop 219Converted from Brinell
Hardness, Rockwell B 92Converted from Brinell
Hardness, Rockwell C 13Converted from Brinell hardness. Value below normal HRC range, for comparison purposes only.
Hardness, Vickers 207Converted from Brinell
Tensile Strength, Ultimate 670 MPa
Tensile Strength, Yield 435 MPa
Elongation at Break 25.5 %in 50 mm
Reduction of Area 56 %
Modulus of Elasticity 205 GPaTypical for steel
Bulk Modulus 160 GPaTypical for steel
Poissons Ratio 0.29Calculated
Machinability 70 %annealed and cold drawn. Based on 100% machinability for AISI 1212 steel.
Shear Modulus 80.0 GPaTypical for steel
Izod Impact 87.0 J
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000223 ohm-cm
@Temperature 20.0 °C
specimen hardened and tempered
 0.0000271 ohm-cm
@Temperature 100 °C
specimen hardened and tempered
 0.0000342 ohm-cm
@Temperature 200 °C
specimen hardened and tempered
 0.0000529 ohm-cm
@Temperature 400 °C
specimen hardened and tempered
 0.0000786 ohm-cm
@Temperature 600 °C
specimen hardened and tempered
 0.0001103 ohm-cm
@Temperature 800 °C
specimen hardened and tempered
 0.0001171 ohm-cm
@Temperature 1000 °C
specimen hardened and tempered
 0.0001222 ohm-cm
@Temperature 1200 °C
specimen hardened and tempered
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.477 J/g-°C
@Temperature >=100 °C
 0.523 J/g-°C
@Temperature 150 - 200 °C
 0.837 J/g-°C
@Temperature 750 - 800 °C
Thermal Conductivity 30.1 W/m-K
@Temperature 1200 °C
 40.7 W/m-K
@Temperature 300 °C
 42.7 W/m-K
@Temperature 100 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.27 - 0.33 %
Chromium, Cr 0.75 - 1.2 %
Iron, Fe 97.1 - 98.38 %As remainder
Manganese, Mn 0.30 - 0.70 %
Molybdenum, Mo 0.15 - 0.25 %
Phosphorus, P <= 0.035 %
Silicon, Si 0.15 - 0.35 %
Sulfur, S <= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 4130 Steel, normalized at 870°C (1600°F)
AISI 4130 Steel, annealed at 865°C (1590°F)
AISI 4130H Steel, annealed at 865°C (1590°F)
AISI 4130 Steel, annealed at 865°C (1585°F), furnace cooled 11°C (20°F)/hour to 680°C (1255°F), air cooled, 25 mm (1 in.) round
AISI 4130 Steel, normalized at 870°C (1600°F), air cooled, 25 mm (1 in.) round

M4130Y / 7510

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.