MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Polysolvan O 50000882 Glycolic acid-n-butyl ester
Categories: Fluid; Solvent

Material Notes: CAS Number: 7397-62-8

Product description: Polysolvan® O (Poly O) is a colorless liquid with a very faint, ester-like odor. It contains no ethanol. Polysolvan® O is miscible with the common organic solvents, but only partially miscible with water. In view of the thermal stability of Polysolvan® O as a “2-hydroxy ester”, reactions such as glycolide formation, transesterification, saponification and etherification are likely at elevated temperatures, especially at boiling point (180 °C). The effect of the resultant changes is an extension of the boiling range upwards.
Dissolving power: Polysolvan® O has excellent dissolving power for polyvinyl acetates, polyvinyl butyrals, vinyl acetate/vinyl chloride/dicarboxylic acid copolymers, nitric acid esters of cellulose (nitrocellulose, celluloid), cellulose ethers, chlorinated rubber, many natural and synthetic resins and most oils and plasticizers.
The following substances are sparingly soluble: Manila copal, shellac, acetic acid esters of cellulose (cellulose acetate), polystyrene (painted articles), indene resin and alkyd resins modified with oleic acid or fatty acid.
Polysolvan® O does not dissolve: Dammar, rubber, bitumen, aldehyde resins, polyisobutylene, painted articles made of polyvinyl chloride (not post-chlorinated) and polyvinyl carbazole, polymethacrylates and polyacrylates.

Applications: Because of its very low volatility Polysolvan® O is used chiefly as a paint additive in the form of a highly effective flow agent. When added in amounts of 3-5 % it gives nitrocellulose lacquers excellent gloss and smooth flow properties. To produce a higher gloss the amount of Polysolvan® O in leather lacquers based on nitrocellulose can be increased. Because of its faint odor Polysolvan® O is also used in brush-applied paints. Although Polysolvan® O hardly dissolves cellulose acetate at all, it can be added to cellulose acetate paints to prevent blushing at high relative humidity. Similarly it is used as a paint additive in alkyd resin and oil paints. The occasionally severe wrinkling of various oil paints can be largely prevented by an addition of 1 – 2 % Polysolvan® O. The addition of Polysolvan® O as a high-boiling solvent to stoving finishes effects uniform flow of the paint film. Polysolvan® O is also employed in the manufacture of printing inks, where extremely faint odor, high boiling point and low volatility are of particular importance. The high dilutability of Polysolvan® O has a beneficial effect in all applications. A highly successful use of the product is in lowering the minimum film-forming temperature (DIN 53 787) of polyvinyl acetate dispersions. When Polysolvan® O is added, it might happen that initial thickening occurs as a result of partial dissolving of the polymer particles; slow addition is therefore recommended. Furthermore it is advisable first to emulsify Polysolvan® O with an equal quantity of water.

Information provided by Celanese Corporation.

Key Words: glycolic acid-n-butyl ester; butyl glycollate; n-butyl glycollate; butyl glycolate; n-butyl glycolate; 1-butanol, glycolic acid ester; C6H12O3; CH3CH2CH2CH2OOCCH2OH
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.015 - 1.023 g/ccDIN 51 757, method D
Density 0.00558 g/ccVapor density
Water Absorption 25 %
Solubility in Water 4.6 %
Viscosity 5.23 cP
@Temperature 20.0 °C
Molecular Weight 132.16 g/mol
Vapor Pressure 0.00130 bar
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 4.00e+6 ohm-cm
Dielectric Constant 13DIN 53 484
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 373 J/g
@Pressure 0.101 MPa
Specific Heat Capacity 2.10 J/g-°C
@Temperature 20.0 °C
Melting Point <= -20.0 °C
Boiling Point 180 °C
@Pressure 0.101 MPa
Flash Point 75.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.425 - 1.427
@Temperature 20.0 °C
nD; DIN 51 423, part 2
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
Evaporation18 wt%DIN 53 249, dipentene
Evaporation number460DIN 53 170

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Poly-L-lactide (PLLA)
Celanese Butoxyl® 50000872 3-Methoxy-n-Butylacetate
Zeus Absorv® Poly(L-lactide) (PLLA) Bioabsorbable Polymer
Flakeboard
Overview of materials for High Density Polyethylene (HDPE), Injection Molded

WCELAN952 / 178023

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.