MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Uniprene® UN-2598A Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Injection Rate: Fast

Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads

Forms: Pellets

Processing Method: Extrusion; Injection Molding

Extrusion Notes: Screw Speed: 30 to 100 rpm

Information Provided by Teknor Apex

Key Words: TPV
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D792
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 201 second; ASTM D2240
Tensile Strength at Break 450 psiASTM D412
Elongation at Break 400 %ASTM D412
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 344 - 416 °F
Middle Barrel Temperature 354 - 426 °F
Front Barrel Temperature 364 - 436 °F
Nozzle Temperature 374 - 446 °F
Zone 1 330 - 400 °F
Zone 2 340 - 410 °F
Zone 3 350 - 420 °F
Zone 5 360 - 430 °F
Die Temperature 374 - 440 °F
Melt Temperature 374 - 446 °FProcessing Temperature
Mold Temperature 95.0 - 140 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 125 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 120 rpm
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Elastamax™ XL 0234-1 SEBS-Based Thermoplastic Elastomer
Barlog Plastics KEBAFLEX SG 25 A.1 TPE-S, Shore A25, natural
ExxonMobil Santoprene® 8211-25 Thermoplastic Elastomer
AlphaGary Evoprene™ G 3290 SEBS Thermoplastic Elastomer
AdvanSource Biomaterials ChronoPrene™ 25A Thermoplastic Rubber Elastomer

PTEKNO891 / 129072

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.