MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Dover Chemical PARA-NONYLPHENOL EG
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Nonylphenol EG is a special grade of nonylphenol to be used in amine cured epoxies. Use in amine epoxies gives improved color versus use of standard Nonylphenol. Typical properties are the same as standard nonylphenol. Applications include: surfactants, TNPP, Phenolic resins, rubber chemistry, PVC, Epoxy resins, and Miscellaneous

Information provided by DoverChem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.947 g/cc
@Temperature 25.0 °C
Viscosity 1500 cP
@Temperature 25.0 °C
Molecular Weight 220 g/mol
ASTM Color <= 50APHA
 
Thermal PropertiesOriginal ValueComments
Pour Point 35.0 °F
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %
 
Descriptive Properties
AppearanceClear, substantially free from suspended matter
Hydroxyl Value240-255
Ortho NP, %<10
PNP, %>90

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDOVER002 / 217621

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.