MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ITW Devcon® Floor Patch™ Epoxy Resurfacer
Categories: Polymer; Thermoset; Epoxy

Material Notes: Self leveling, filled epoxy system for repairing heavily spalled concrete floors. Uses: For repairing heavily spalled, fragmented concrete floors. A minimum thickness of 0.25" is recommended. Features: Self-leveling, Bonds to metal and concrete, Low shrinkage, Resists industrial chemicals, Mixes easily.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 16.7 lb/galCured
Solids Content 100 %
Viscosity 5000 cPMixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
Compressive Strength 19480 psiASTM D695
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 50.0 - 90.0 °FApplication Temperature
Cure Time 24.0 hour
@Temperature 24.0 °C
Functional cure
 168 hour
@Temperature 24.0 °C
As Tested
Pot Life 40.0 min
@Temperature 23.9 °C
 
Descriptive Properties
Aggregate/Liquid Ratio1:1.25Resin/hardener. By volume
 1:3Resin/Hardener. By weight
Chemical/Solvent ResistanceAmmonia: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Chlorinated Solvent: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric Acid 10%: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Kerosene: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Methanol: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 10%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric Acid 10%: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Toluene: poor30 day immersion at 75°F. Sample cured 7 days at RT
ColorGrayCured
Coverage15.8 ft²Cured. @ 1/4"
Mix Ratio by volume4.2:1Resin/Hardener
Mix Ratio by weight4.5:1Resin/Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWD9213 / 239722

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.