MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Unipetrol 70/100 Road Bitumen
Categories: Fluid

Material Notes: At normal temperatures, road bitumens are semi-solid to solid homogeneous bitumen substances. They are produced as residual fractions of vacuum distillation of the atmospheric crude oil residual fraction, by blowing crude oil residual fractions or by mixing oxidized asphalts with crude oil residual fractions. Road bitumens are used for the production of penetration macadams, packaging mixtures, cast asphalts, for the construction and maintenance of asphalt roads, sidewalks, for the bottom layer of roads and in the production of asphalt concrete.

Information provided by Unipetrol RPA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Penetration >= 46remnant
 
Thermal PropertiesOriginal ValueComments
Ring & Ball Softening Point >= 45.0 °Cafter aging @ 163°C
 43.0 - 51.0 °C
 
Descriptive Properties
Breaking Point °C-10
Increase in Softening Point (°C)11

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Asphalt
Lucobit Luxbit® Hard Bitumen
Concrete, 1-4 Dry
Unipetrol 50/70 Road Bitumen
Unipetrol 160/220 Road Bitumen

PUNIP085 / 82945

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.