DOW LDPE 503A resin is used for liner film and other packaging applications that require optical clarity. It contains medium levels of slip additive and low levels of antiblock additive. It complies with U.S. FDA regulation 21 CFR 177.1520 (c) 2.1 for food contact applications. The regulation should be consulted for complete details. Film properties below based on a film thickness of 40 µm. Data provided by Dow Chemical. |