MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmodur® L 67 BA Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Aromatic polyisocyanate based on toluene diisocyanate. In combination with various Desmophen® grades or other hydroxyl-bearing substances to formulate air-drying two-component polyurethane coatings.

Properties / Applications: Systems crosslinked with Desmodur® L 67 BA can be used as coatings for furniture, parquet flooring, metal, paper, plastics and mineral substrates.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccDIN EN ISO 2811-3
Volatiles 31 - 35 %31 - 35 %DIN EN ISO 3251
Viscosity 400 - 800 cP400 - 800 cPDIN EN ISO 3219/A.3
 
Thermal PropertiesMetricEnglishComments
Flash Point 30.0 °C86.0 °FDIN EN ISO 1523
 
Descriptive Properties
Color<2Iodine, DIN EN 1557
Content<0.5%Monomeric TDI, DIN EN ISO 10 283
 11.5-11.3%NCO, DIN EN ISO 11 909

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmodur® IL BA Polyurethane
Covestro Desmodur® IL 1451 Polyurethane
Covestro Desmodur® IL 1351 Polyurethane
Covestro Desmodur® IL 1351 51% EA Polyurethane
Covestro Desmodur® IL 1351 51% BA Polyurethane

PCOVEST0358 / 202141

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.