MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain COHRlastic® 440S Silicone Solid/High Temp Silicone Adhesive Pressure Sensitive Tape
Categories: Polymer; Adhesive; Tape; Thermoset; Silicone

Material Notes: Description: Strip-N-Stick® tape provides all the benefits of silicone rubber in an easy-to-apply, pressure-sensitive adhesive tape form. Compressible and flexible, it can conform to irregular surfaces, wrap over cylinders or be formed to produce right angles. Applications include gasketing, vibration damping, and thermal insulation. The tape reduces the need for expensive die-cut-parts--you don't pay for the center. It also eliminates the high cost of bonding and will be slit to order for 1/2" and up. 440S is a 1/32" thick Shore A 30 durometer silicone solid with high-temperature silicone adhesive. Adhesive temperature range for Silicone PSA is -100°F to +500°F and for Acrylic PSA, -20°F to 300°F. Silicone rubber material type is solid. Adhesive type is silicone. All data based on a 0.03125 inch test sample.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 700 psiASTM D412
Elongation at Break 650 %ASTM D412
Compressive Strength 45.0 psiCompression Deflection, Compressed to 75% original thickness.; ASTM D1056
Compression Set 30 %
@Temperature 100 °C
Constant Deflection, Compressed 50% for 22 hrs; ASTM D1056
 
Descriptive Properties
ColorLight Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP21TDC-4ND Two component, highly flexibilized epoxy for bonding, sealing and coating
Aremco Pyro-Tape™ 682-CR High Temperature Tape Single-layer Teflon coated fiberglass with a high strength silicone adhesive
Saint-Gobain COHRlastic® 100S Silicone Sponge/High Temp Silicone Adhesive Pressure Sensitive Tape
NanoMas NanoGold™ NTG05IJ05 Conductive Ink
Cotronics Resbond™ 904 Ultra Temp Zirconia Adhesive and Coating

PSTGQZ263 / 68777

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.