MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Marble
Categories: Ceramic

Material Notes: Metamorphic rock with the critical mineral calcite (90-100%). It is formed from limestone.

Property values are typical of Marble used in construction. Actual property values will vary from sample to sample.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.37 - 3.20 g/cc0.0856 - 0.116 lb/in³
Moisture Expansion 0.0025 %0.0025 %Coarse crystalline; Source: Georgia, USA
Porosity 0.50 - 2.0 %0.50 - 2.0 %
Permeability 1.0e-6 - 0.00101.0e-6 - 0.0010Aggregation property, d (µ = (-log d))
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore H 45 - 5645 - 56
Hardness, Mohs 2.0 - 4.32.0 - 4.3
Abrasive Hardness 7.0 - 427.0 - 42
Tensile Strength, Ultimate 7.00 - 20.0 MPa1020 - 2900 psi
Modulus of Elasticity 60.0 GPa8700 ksi
Modulus of Rupture 0.00410 - 0.0276 GPa0.595 - 4.00 ksi
Transverse Strength 4.00 - 27.0 MPa580 - 3920 psi
Compressive Strength 68.9 - 241 MPa10000 - 35000 psi
Impact Toughness 0.787 - 9.06 cm/cm²2.00 - 23.0 in/in²
 
Thermal PropertiesMetricEnglishComments
CTE, linear 2.70 - 9.00 µm/m-°C
@Temperature 20.0 °C
1.50 - 5.00 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.540 - 1.61 J/g-°C0.129 - 0.385 BTU/lb-°F
Thermal Conductivity 1.30 - 2.90 W/m-K9.02 - 20.1 BTU-in/hr-ft²-°F

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Limestone
Granite
Sandstone, Medium
Basalt
Glass Fiber Reinforced Concrete

BMIN086 / 211

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.