MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Thermx® LED 0201 PCT, 40% Specialty
Categories: Polymer; Thermoplastic; Polyester, TP; Polycyclohexylenedimethylene Terephthalate (PCT); Polycyclohexylenedimethylene Terephthalate (PCT), 40% Glass Reinforced

Material Notes: Thermx LED 0201 is a super white reinforced PCT resin highly suitable for LED applications. The material exhibits high heat resistance, high reflectance stability, high thermal stability, low moisture absorption, and high mechanical properties for injection molding.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.62 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0030 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 73.0 MPa5mm/min; ISO 527-2/1A
Elongation at Break 1.7 %5mm/min; ISO 527-2/1A
Tensile Modulus 6270 MPa50mm/min; ISO 527-2/1A
Charpy Impact Unnotched 32.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 3.20 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 32.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 102 µm/m-°CISO 11359-2
Melting Point 285 °C10°C/min; ISO 11357-1,-2,-3
 
Processing PropertiesOriginal ValueComments
Processing Temperature 100 - 150 °Ccavity
Zone 1 290 - 305 °C
Zone 2 285 - 300 °C
Zone 3 285 - 300 °C
Zone 4 285 - 300 °C
Die Temperature 285 - 295 °C
Melt Temperature 290 - 310 °C
Drying Temperature 95.0 - 100 °C
Dry Time 4.00 - 6.00 hour
Moisture Content <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Thermx® TE3002 BK010 PCT
Celanese Thermx® TE1001 BK010 PCT
Celanese Thermx® CG023 NC010 PCT
Celanese Zenite® 5145L WT010 LCP
Celanese Thermx® TE4004 PCT, 40% Specialty

PHCQ468 / 178923

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.