MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rogers Arlon 55109R028 Silicone Rubber/Fiberglass Laminate
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: cured silicone rubber; Substrate: 162 fiberglass

Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/ccsilicone property, layer 1; Arlon SQA-TMS-024
 1.35 g/cc1.35 g/ccsilicone property, layer 2; Arlon SQA-TMS-024
Thickness 88.9 microns3.50 millayer 1; Arlon SQA-TMS-003
 178 microns7.00 millayer 2; Arlon SQA-TMS-003
 483 microns19.0 milsubstrate; Arlon SQA-TMS-003
 749 microns29.5 miloverall; Arlon SQA-TMS-003
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060silicone property, layer 1; ASTM D2240
 6060silicone property, layer 2; ASTM D2240
Tensile Strength, Ultimate 5.52 MPa800 psisilicone property, layer 1; ASTM D412
 5.52 MPa800 psisilicone property, layer 2; ASTM D412
Elongation at Break 225 %225 %silicone property, layer 1; ASTM D412
 225 %225 %silicone property, layer 2; ASTM D412
Adhesive Bond Strength 0.0545 MPa7.90 psiASTM D624
Tear Strength 15.8 kN/m90.0 pliDie B, layer 1; ASTM D624
 15.8 kN/m90.0 pliDie B, layer 2; ASTM D624
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 17.3 kV/mm440 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 120 min
@Temperature 204 °C
2.00 hour
@Temperature 400 °F
 15.0 min
@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour
@Pressure 50.0 psi,
Temperature 250 °F
Shelf Life 6.00 Month
@Temperature 23.9 °C
6.00 Month
@Temperature 75.0 °F
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon 55096R028 Silicone Rubber/Fiberglass Laminate
Rogers Arlon 56976XA026 Silicone Rubber/Fiberglass Laminate
Rogers Arlon Thermabond® 99180T010 Silicone Rubber/Fiberglass Laminate
Rogers Arlon 51106R015 Silicone Rubber/Fiberglass Laminate
Rogers Arlon 51106R020 Silicone Rubber/Fiberglass Laminate

PARL031 / 79683

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.