MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total Lumicene® mPE M5510 EP Metallocene Polyethylene, Blown Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: This product is a Total Ecosolutions grade.

Lumicene® mPE M5510 EP is a second generation metallocene high density homopolymer polyethylene.

Lumicene® mPE M5510 EP can be processed at high output rates with low extrusion pressure, excellent bubble stability and gauge control in comparison with conventional LLDPE and first generation metallocene based polyethylene. The outstanding stiffness combined with good optical properties brings a significant downgauging potential.

The high density of Lumicene® mPE M5510 EP enables its use in applications with moisture barrier requirements, such as dry food packaging, and brings improved heat resistance, compared to commonly used HDPE.

Lumicene® mPE M5510 EP is suited for many applications in the field of consumer, industrial, food or hygiene packaging such as bags, heavy-duty sacks, automatic packaging specialty film, mailing film and lamination.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.955 g/ccISO 1183
Thickness 40.0 microns
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 27.5 MPaISO 527-3
Film Tensile Strength at Yield, TD 28.0 MPaISO 527-3
Film Elongation at Break, MD 870 %ISO 527-3
Film Elongation at Break, TD 910 %ISO 527-3
Elmendorf Tear Strength, MD 1.10 g/micronISO 6383-2
Elmendorf Tear Strength, TD 9.20 g/micronISO 6383-2
Dart Drop Test 100 gISO 7765-1
Film Tensile Strength at Break, MD 57.0 MPaISO 527-3
Film Tensile Strength at Break, TD 45.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 134 °CISO 11357
Vicat Softening Point 133 °CISO 306
 
Optical PropertiesOriginal ValueComments
Haze 24 %ISO 14782
Gloss 40 %at 45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 - 230 °CBlow Molding
Melt Temperature 210 °CExtrusion
Die Opening 0.0800 - 0.280 cm
Blow-up Ratio (BUR) 1.5 - 4.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total Lumicene® mPE M 4707 EP Metallocene Polyethylene, Blown Film
Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film
Total Lumicene® mPE M 5220 High Density Polyethylene, Blow Molding
Total Lumicene® MR10MX0 Metallocene Random Copolymer Polypropylene, Injection Molding and Injection Blow Molding
Total Lumicene® mPE M 2735 S01 Metallocene Polyethylene, Cast Film

PTOTAL784 / 130509

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.