MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Asahi Kasei Leona™ 91G60 Polyamide 66, MF Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Applications: Automotive parts, electrical & electronic parts, parts for office furnishings. 90G series has enhanced stiffness, excellent surface appearance, and good moldability.

Information provided by Asahi Kasei Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.72 g/ccDry as Molded; ASTM D792
Density 1.72 g/ccDry as Molded; ISO 1183
Moisture Absorption at Equilibrium 1.0 %
@Temperature 23.0 °C
50% RH; ISO 62
 1.0 %
@Temperature 23.0 °C
50% RH
Linear Mold Shrinkage, Flow >= 0.0020 cm/cmAsahi Kasei
Linear Mold Shrinkage, Transverse >= 0.0080 cm/cmAsahi Kasei
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 88Conditioned at 50% RH; ISO 2039
 95Dry as Molded; ISO 2039
Hardness, Rockwell R 117Conditioned at 50% RH; ISO 2039
 120Dry as Molded; ISO 2039
Tensile Strength at Break 142 MPaConditioned at 50% RH; ISO 527
 173 MPaDry as Molded; ISO 527
Tensile Strength 150 MPaConditioned at 50% RH; ASTM D638
 183 MPaDry as Molded; ASTM D638
Elongation at Break 3.0 %Dry as Molded; ISO 527
 5.4 %Conditioned at 50% RH; ISO 527
Tensile Modulus 16400 MPaConditioned at 50% RH; ISO 527
 17500 MPaDry as Molded; ISO 527
Flexural Strength 235 MPaConditioned at 50% RH; ISO 178
 255 MPaDry as Molded; ISO 178
Flexural Modulus 15700 MPaConditioned at 50% RH; ISO 178
 16400 MPaDry as Molded; ISO 178
Izod Impact, Notched 63.0 J/mDry as Molded; ASTM D256
 64.0 J/mConditioned at 50% RH; ASTM D256
Charpy Impact, Notched 6.00 kJ/m²Dry as Molded; ISO 179
 6.10 kJ/m²Conditioned at 50% RH; ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 µm/m-°CDry as Molded; ASTMD 696
Deflection Temperature at 0.46 MPa (66 psi) 217 °CDry as Molded; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 200 °CDry as Molded; ISO 75
Flammability, UL94 HB
@Thickness 0.750 mm
Dry as Molded

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Pocan® T 7391 POS151 900044 PBT+PET, 45% Glass Fiber Filled
Envalior Durethan® BKV 240 H2.0 XCP 901510 Nylon 6 (PA6), 40% Glass Fiber Reinforced, Dry
Envalior Durethan® BKV 50 H2.0 901510 Nylon 6 (PA6), 50% Glass Fiber Reinforced, Dry
Asahi Kasei Leona™ 13G50 Polyamide 66, GF Reinforced
Mitsubishi Chemical Advanced Materials Duratron™ T4203 PAI Extruded Polyamide-imide

PASAHI8150 / 221177

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.