MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Versalis Sinkral® PD L 322 ABS Resin  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Sinkral PD L 322 by continuous mass, is a general purpose, high flow injection molding grade having good impact resistance coupled with an excellent gloss.

Applications: Widely used in the small and large household appliance sector, vacuum cleaners, toys, telephones and consumer electronics.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccISO 1183
Water Absorption 0.30 %
@Time 86400 sec
ASTM D570
Melt Flow 23 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 109ISO 2039/2
Tensile Strength at Break 45.0 MPaASTM D638
Elongation at Break 20 %ASTM D638
Flexural Strength 69.0 MPaASTM D790
Flexural Modulus 2350 MPaASTM D790
Izod Impact, Notched 50.0 J/m
@Thickness 3.20 mm,
Temperature -40.0 °C
ISO 180/4A
 70.0 J/m
@Thickness 3.20 mm,
Temperature -20.0 °C
ISO 180/4A
 100 J/m
@Thickness 3.20 mm,
Temperature 0.000 °C
ISO 180/4A
 170 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ISO 180/4A
Izod Impact, Notched (ISO) 6.00 kJ/m²
@Thickness 4.00 mm,
Temperature -40.0 °C
ISO 180/1A
 13.0 kJ/m²
@Thickness 4.00 mm,
Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
DIN 53453
 NB
@Temperature -40.0 °C
DIN 53453
Charpy Impact, Notched 9.00 kJ/m²
@Temperature 23.0 °C
DIN 53453
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohmIEC 60093
Dielectric Constant 3.1
@Frequency 1000 Hz
dry; IEC 60250
Dielectric Strength 30.0 kV/mmIEC 60243
Dissipation Factor 0.015
@Frequency 1000 Hz
dry; IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°CASTM D696
Thermal Conductivity 0.170 W/m-KASTM C177
Vicat Softening Point 96.0 °C
@Load 5.10 kg
ISO 306/B 120
 99.0 °C
@Load 1.02 kg
ISO 306/A 120
Flammability, UL94 HB
@Thickness 1.50 mm
Glow Wire Test 650 °C
@Thickness 3.00 mm
IEC 60695-2-1
Shrinkage 0.40 - 0.60 %Internal method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical TR-558 Transparent ABS, Humidity Resistance, Natural and Colored Pellets
INEOS Styrolution Terluran® GP-35 ABS
INEOS Styrolution Polystyrol 454 C GR 2 PS
Versalis SINKRAL PD F332 ABS, Heat Stabilized

PENG167 / 124561

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.