MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Unifrax Fiberfrax® Fibermax® Mat Ceramic Fiber Insulator
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Fibermax Mat is a high-temperature, flexible mat product that is lightweight (1.5 lb/ft3 density) and highly resilient. It is composed entirely of Fibermax polycrystalline mullite fibers to produce a product that is high-temperaure (1650°C / 3000°F) resistant and virtually shot-free.

Fibermax Mat contains no organic binders or other additives which cause outgassing fumes or associated problems. In addition to exhibiting excellent resistance to attack from most corrosive agents (exceptions include hydrofluoric acid, phosphoric acid and strong alkalies), Fibermax fiber also resists oxidation and reduction.

    Typical Applications
  • Expansion joint packing
  • Burner wraps
  • Batten strips with fiber modules
  • Aluminum homogenizing furnace linings

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.00 g/cc
Density 1.50 lb/ft³
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.246 J/g-°C
@Temperature 1093 °C
Melting Point 1870 °C
Maximum Service Temperature, Air 1566 °CRecommended Operating Temperature
 
Component Elements PropertiesOriginal ValueComments
Al2O3 72 %
CaO 0.050 %
Fe2O3 0.020 %
MgO 0.050 %
SiO2 27 %
TiO2 0.0010 %
 
Descriptive Properties
ColorWhite
Fiber Diameter (microns)2-3.5
Fiber Surface Area (m2/g)7.65
Leachable Chlorides (ppm)11
Na2O3 (%)0.1
Temperature Grade (°C)1650

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator
Unifrax Fiberfrax® Fibermat® Blanket Ceramic Fiber Insulator
Unifrax Fiberfrax® Durablanket® 2600 Ceramic Fiber Insulator
Pyrotek Fiber Seal Y-1 Ceramic fiber paper
Sinotek Materials BG Board Ceramic Fiber Board, White, Heat Insulation Material

CUNIF025 / 97797

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.