MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPH 3740WR Polypropylene, High Flow Nucleated Homopolymer Injection Molding
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Easy Flow TOTAL Polypropylene 3740WR exhibits exceptionally easy flow characteristics.

FDA. 3740WR complies with all applicable FDA and USDA regulations and may be used under these provisions for food contact and packaging.

Recommended Applications. TOTAL Polypropylene 3740WR is recommended for injection molding medical applications requiring high stiffness and good gamma radiation stability up to 50 kGy.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/ccASTM D1505
Melt Flow 20 g/10 minASTM D1238, L
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75ASTM D1706
Tensile Strength, Yield 37.0 MPaASTM D638
Elongation at Yield 7.0 %ASTM D638
Tensile Modulus 1655 MPaASTM D638
Flexural Modulus 1725 MPaASTM D790
Izod Impact, Notched 16.0 J/mASTM D256A
Impact Test 0.420 ft-lb
@Thickness 3.17 mm
Drop Impact; API
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 116 °CASTM D648
 
Compliance PropertiesOriginal ValueComments
USDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Flint Hills P5M6K-080 Polypropylene Random Copolymer
LyondellBasell Pro-fax PF531 Polypropylene Homopolymer, Radiation Resistant
ExxonMobil Exceed™ PP9074MED Polypropylene Homopolymer
Flint Hills P9M7R-056 Specialty Homopolymer Polypropylene
LyondellBasell Pro-fax PD702 Polypropylene Homopolymer, High Flow

PTOTAL816 / 130541

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.